Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.401 g/cc | 0.0145 lb/in³ | ASTM D1667 |
Saint-Gobain Korel® K30-25 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |