Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.350 - 0.410 g/cc | 0.0126 - 0.0148 lb/in³ | True, 3M QCM 14.24.6 |
3M HGS4000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Density | 0.350 - 0.410 g/cc | 0.0126 - 0.0148 lb/in³ | |
3M S38 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.350 - 0.410 g/cc | 0.0126 - 0.0148 lb/in³ | |
3M S38HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.350 - 0.410 g/cc | 0.0126 - 0.0148 lb/in³ | True, 3M QCM 14.24.6 |
3M HGS5000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |