Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 11.4 g/cc | 0.412 lb/in³ | |
China Tungsten YT14 Tungsten Carbide for Cutting Tools High strength in use and good impact & shock resistance, yet lower than YT5,Rough turning and rough milling of carbon steel and alloy steel during continuous cutting or medium to fine turning of the.. |
|||
Density | 11.4 g/cc | 0.412 lb/in³ | |
China Tungsten ZP20 Tungsten Carbide High in impact resistance and strength in use. Roughing and semi-finishing of steel, cast steel, forgeable cast iron and nodular cast iron.Information provided by China Tungsten |