Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 13.4 g/cc | 0.484 lb/in³ | |
Wieland Auropal 50 Casting Alloy Gold-silver casting alloyApplications: inlays/onlays, crowns, short span bridges, acrylic veneeringDental |
|||
Density | 13.4 - 13.7 g/cc | 0.484 - 0.495 lb/in³ | |
China Tungsten YG20C Tungsten Carbide for Dies and Wear Part Making For cold forging, punching pressing dies for standard components bearings and tools industries etc; and for punching dies for bullet heads and cartridges.Information provided by China Tungsten |
|||
Density | 13.4 g/cc | 0.484 lb/in³ | |
CMW® ELKONITE 4050 tungsten, high silver ELKONITE® 4050 is a high silver material that uses a special tungsten powder. It is made by the press-sinter-infiltrate method. It was developed especially for use as a combination current carrying.. |
|||
Density | 13.4 - 13.7 g/cc | 0.484 - 0.495 lb/in³ | |
China Tungsten YG20 Tungsten Carbide for Dies and Wear Part Making For fabricating of stamping dies for watch parts, spring plates of musical instruments, batters jars, small sized steel balls, screws, screwcaps, etc; and for press plates for hot rolling of twist d.. |