Polymer Property : Density = 0.5123 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 14.18 g/cc
0.5123 lb/in³
CMW® ELKONITE® 5W3 Tungsten Copper material ASTM B702, Class C, infiltrated
For arcing and current carrying electrical contacts; power transformer contacts.Information provided by CMW Inc.
Density 14.18 g/cc
0.5123 lb/in³
Cadi 5WC Tungsten Copper
Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company.