Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 14.77 g/cc
0.5336 lb/in³
CMW® ELKONITE® 35S Silver Tungsten contact material ASTM B631, Class B, infiltrated
For arcing and current carrying electrical contacts; household and power circuit breakers.Information provided by CMW Inc.
Density 14.77 g/cc
0.5336 lb/in³
Cadi 35WS Tungsten Silver
Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company.