Density 14.7 - 15.3 g/cc
0.531 - 0.553 lb/in³
H.C. Starck WCu 75/25 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
Density 15.0 - 15.3 g/cc
0.542 - 0.553 lb/in³
China Tungsten YG3X Tungsten Carbide for Dies and Wear Part Making
For drawing of steel non-ferrous metal and alloy wire of