Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.562 g/cc | 0.0203 lb/in³ | |
3M Cushion-Mount™ E1840 Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Density | 0.562 g/cc | 0.0203 lb/in³ | |
3M Cushion-Mount™ E1860 Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |