Polymer Property : Density = 0.5679 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 15.72 g/cc
0.5679 lb/in³
CMW® ELKONITE® 20S Infiltrated Tungsten Silver Contact Material ASTM B531, Class A, infiltrated
For electrical contacts resistant to arcing and welding in circuit breakers, etc.Information provided by CMW Inc.