Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.593 g/cc | 0.0214 lb/in³ | |
Pyrotek Wollite 37 Insulating Castable Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting c.. |
|||
Density | 0.593 g/cc | 0.0214 lb/in³ | |
Pyrotek Z-5 Fiberglass Fabric Fiberglass, coarse textile fiber. Woven fabric.Information provided by Pyrotek. |
|||
Density | 0.593 g/cc | 0.0214 lb/in³ | ASTM C134 |
BNZ Materials BNZ-23 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.593 g/cc | 0.0214 lb/in³ | ASTM C134 |
BNZ Materials BNZ-24 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.593 g/cc | 0.0214 lb/in³ | |
BNZ Materials 2337LI Insulating Aggregate BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i.. |