Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.625 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.625 - 0.657 g/cc
0.0226 - 0.0237 lb/in³
Pyrotek AL-THERM 2100H Vacuum formed refractories for use with modular hot top systems
Pyrotek offers a variety of vacuum formed products composed from Al-Therm 2100H. These alumina-silicate fibers feature a unique inorganic binder system and are custom designed to shapes which are f..
Density 0.625 g/cc
0.0226 lb/in³
Pyrotek IR-3 Fiber Seal Pre-cut Gasket
A felt-like material which expands between 350°C and 540°C.Information provided by Pyrotek.
Density 0.625 g/cc
0.0226 lb/in³
Pyrotek IR-3 Low-Temperature Felt
Felt-like material which expands between 350°C and 540°C.Custom Rolls:3 & 6 mm thickApplicationsCompressible gasketing Collector bar seals Siphon gaskets Flange gaskets Information provided by Pyr..
Density 0.625 g/cc
0.0226 lb/in³
ASTM D1505
PolyOne OnColor™ 30BKA488 Black Polyvinyl Chloride, Unspecified (PVC, Unspecified)
Dispersion Note: On a scale in which 1 represents an excellent dispersion and 5 a poor dispersion. Heat Stability Note: Under normal processing conditions there is normally no significant color chan..
Density 0.625 g/cc
0.0226 lb/in³
Zircar Zirconia Buster M2-35 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..
Density 0.625 g/cc
0.0226 lb/in³
Nominal
Unifrax FyreWrap® XFP® Expanding Paper
FyreWrap® XFP® Expanding Paper is a flexible, lightweight, high-temperature intumescent mat that expands up to three times its thickness when exposed to temperatures above 620°F (325°C). In the..
Density 0.625 g/cc
0.0226 lb/in³
Zircar Zirconia Buster M2-35 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..
Density 0.625 g/cc
0.0226 lb/in³
Trelleborg AEM Eccofloat® DS-39/11500 Syntactic Foam
DS Grade syntactic foams combine lightweight glass Eccospheres® with multifunctional epoxy resin to produce ultra-high strength-to-weight materials for high-performance, deep sea applications inclu..
Density 0.625 g/cc
0.0226 lb/in³
Trelleborg AEM Eccofloat® TG-39/10000 Syntactic Foam
TG Grade syntactic foams are lightweight and economical for building manned and remote operating vehicles. The foams are also used to manufacture mine neutralization systems because of their zero ma..
Density 0.625 g/cc
0.0226 lb/in³
ASTM C134
BNZ Materials PA 20 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Density 0.625 g/cc
0.0226 lb/in³
ASTM C134
BNZ Materials Zelieblok 1900S Structural Ceramic Insulation
Information provided by BNZ Materials Inc.