Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 17.4 - 17.8 g/cc | 0.629 - 0.643 lb/in³ | |
H.C. Starck HPM 1760 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Density | 17.4 - 17.8 g/cc | 0.629 - 0.643 lb/in³ | |
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the custo.. |
|||
Density | 17.4 g/cc | 0.629 lb/in³ | |
CMW® ELKONITE 2088 very high refractory, tungsten, silver ELKONITE® 2088 has a very high refractory content and is not considered in the normal family of make and break contacts. It is used in special applications where weight or hardness together with co.. |
|||
Density | 17.4 g/cc | 0.629 lb/in³ | |
CMW® ELKONITE® 2188 Infiltrated Tungsten Silver Contact Material High wear resistance and reliability.Information provided by CMW Inc. |