Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.570 - 0.630 g/cc | 0.0206 - 0.0228 lb/in³ | True, 3M QCM 14.24.6 |
3M HGS10000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Density | 0.570 - 0.630 g/cc | 0.0206 - 0.0228 lb/in³ | True, 3M QCM 14.24.6 |
3M HGS18000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Density | 0.570 - 0.630 g/cc | 0.0206 - 0.0228 lb/in³ | |
3M iM30K Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.570 - 0.630 g/cc | 0.0206 - 0.0228 lb/in³ | |
3M S60HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.570 - 0.630 g/cc | 0.0206 - 0.0228 lb/in³ | |
3M S60 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |