Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.480 - 0.640 g/cc | 0.0173 - 0.0231 lb/in³ | |
Pyrotek PTB 2200 Structural Board ApplicationsCaster tips Small machined nozzles Slotted caster tips AdvantagesHigh strength Resistant to thermal shock Easily machined Non-wetting to molten non-ferrous metals Low thermal mass High t.. |