Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.679 - 1.17 g/cc | 0.0245 - 0.0423 lb/in³ | Average value: 1.14 g/cc Grade Count:63 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |