Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | <= 0.792 g/cc | <= 0.0286 lb/in³ | 2nd Grade |
Kazanorgsintez PC-003 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez |
|||
Density | 0.792 g/cc @Temperature 15.6 °C |
0.0286 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Varsol™ DX 140 Naphtha Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil |