Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.809 g/cc @Temperature 15.0 °C |
0.0292 lb/in³ @Temperature 59.0 °F |
|
ExxonMobil Mobilarma 245 Mobilarma 200 Series products are premium quality rust preventive materials designed to protect metal surfaces from rust and corrosion. They are formulated using light-bodied petroleum solvents with.. |
|||
Density | 0.809 g/cc @Temperature 15.0 °C |
0.0292 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Exxsol™ D220/230 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.809 g/cc @Temperature 15.0 °C |
0.0292 lb/in³ @Temperature 59.0 °F |
|
ExxonMobil Mobilarma 245 Mobilarma 200 Series products are premium quality rust preventive materials designed to protect metal surfaces from rust and corrosion. They are formulated using light-bodied petroleum solvents with.. |