Polymer Property : Density = 0.830 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.790 - 0.830 g/cc
0.0285 - 0.0300 lb/in³
RP-17617
Solvay RHODOLINE® 581B Surfactant
Description: Mineral oil defoamers for high PVC systems Chemical Name: DEFOAMERCAS: 64742-47-8Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility(2% in DI Water): Coarse Di..
Density 0.780 - 0.830 g/cc
0.0282 - 0.0300 lb/in³
ASTM D4052
ExxonMobil Jayflex™ 220 Aliphatic Hydrocarbon Plasticizer
Availability: North AmericaCAS Number: 64742-47-8Information provided by ExxonMobil