Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.862 g/cc | 0.0311 lb/in³ | ASTM D792 |
Dow Engage® ENR 7467.00 Ethylene-Butene Copolymer Description: ENR 7467.00 is a high performance ethylene-butene copolymer, offering superior impact properties for more demanding TPO applications. The polymer has very low crystallinity and is avail.. |
|||
Density | 0.862 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Velocite 10 The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra.. |
|||
Density | 0.862 g/cc | 0.0311 lb/in³ | |
ConocoPhillips 32 Super Hydraulic Oil Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, .. |
|||
Density | 0.862 g/cc | 0.0311 lb/in³ | |
ConocoPhillips Hydroclear® 46 Refrigerant Oil Description: Conoco Hydroclear Refrigerant Oil is a high-quality ammonia refrigeration compressor lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Refrigerant Oil is spe.. |
|||
Density | 0.862 g/cc | 0.0311 lb/in³ | |
ConocoPhillips Hydroclear® MV32 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Density | 0.862 g/cc | 0.0311 lb/in³ | |
ConocoPhillips 22 Super Hydraulic Oil Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, .. |
|||
Density | 0.862 - 0.910 g/cc | 0.0311 - 0.0329 lb/in³ | Average value: 0.885 g/cc Grade Count:16 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a.. |
|||
Density | 0.862 g/cc | 0.0311 lb/in³ | |
ConocoPhillips 32 Ultra-Clean Super Hydraulic Oil Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1.. |
|||
Density | 0.862 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Velocite 10 The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra.. |