Physical Properties Metric English Comments
Density 0.894 g/cc
0.0323 lb/in³
ASTM D1505
Flint Hills P5M2Z-012 Polypropylene Random Copolymer
Features: Good contact clarity. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: film and blow moldingInformation Provided by Flint Hills Resources
Density 0.894 g/cc

@Temperature 15.0 °C
0.0323 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil 40 Exxon XD-3
Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d..
Density 0.894 g/cc

@Temperature 15.0 °C
0.0323 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil 40 Exxon XD-3
Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d..
Density 0.894 g/cc
0.0323 lb/in³
ConocoPhillips 460M Gear Oil AGMA Lubricant No.7EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
Density 0.894 g/cc
0.0323 lb/in³
ConocoPhillips Hydroclear® 460 7 EP gear Oil
Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary addi..
Density 0.894 g/cc
0.0323 lb/in³
ConocoPhillips Inca® 460 Oil, AGMA No. 7 Comp.
Description: Conoco Inca Oil is a high-quality compounded lubricant recommended for use in heavily loaded industrial and automotive worm gears and bearings operating at moderate to high temperatures..
Density 0.894 g/cc
0.0323 lb/in³
ConocoPhillips 460 Gear Oil AGMA Lubricant No. 7 EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..