Polymer Property : Density = 0.895 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.865 - 0.895 g/cc
0.0313 - 0.0323 lb/in³
RP-17617
Solvay RHODOLINE® 681-F Surfactant
Description: Mineral oil defoamers for high PVC systems.Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: For best results, RHODOLINE© 681-F should be used as received. As..