Density 0.8965 g/cc
0.03239 lb/in³
ASTM D792
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP)
AFFINITY™ PF 1140G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to be used in a variety of demanding applications including form-fill-seal packaging and fre..