Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.9055 g/cc | 0.03271 lb/in³ | ASTM D792-91 |
Multibase Multi-Pro® 0110 X Natural Polypropylene This product is suitable for moldings incorporating high temperature requirements. This material is specially formulated to be resistant to Copper, but is also resistant to most metals.Data provide.. |
|||
Density | 0.9055 g/cc | 0.03271 lb/in³ | ASTM D792 |
Dow FLEXOMER™ DFDA-1010 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1010 NT 7 is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins .. |