Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D4883 |
Eastman D4056-P Polyethylene
(discontinued **) Polyethylene D4056-P is a natural low density material with an 80 melt index.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no lon.. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 10A Octene VLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealability, easy processability, excellent clarity.Applications: Blending resin for improved toughness.Data provided by the manufacturer. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 10B Octene VLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealability, excellent dart impact, excellent clarity.Applications: Co-extrusion.Data provided by the manufacturer. |
|||
Density | 0.911 g/cc @Temperature 20.0 °C |
0.0329 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell DPNB Dipropylene glycol normal butyl ether Information provided by Lyondell. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D1475 |
Humiseal 1A33 Urethane Conformal Coating Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL.. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D1475 |
Humiseal 1B31 Acrylic Conformal Coating Humiseal 1B31 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C ApprovedPasses thermal shock test (MI.. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D792 |
Ineos H44N-00 Polypropylene Homopolymer H44N-00 is a high flow rate, nucleated polypropylene homopolymer designed for compounding and injection molding applications. The grade benefits from a high stiffness and isotropic shrinkage to help.. |
|||
Density | 0.911 g/cc @Temperature 20.0 °C |
0.0329 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell PMP Propylene glycol methyl ether propionate Information provided by Lyondell. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D1505 |
Westlake EC4056AA Low Density Polyethylene WESTLAKE low-density polyethylene EC4056 is a natural low density material with an 80 melt index.FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All in.. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ISO 1183 |
ExxonMobil Exxtral™ CNU 017 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by high flow, high stiffness, low odor and emissions that is typically used automotive air conditioning units.Availabili.. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D792 |
Dow AFFINITY™ PT 1409 Polyolefin Plastomer (POP) AFFINITY™ PT 1409 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies from Dow Plastics. Resin blended with 20 wt% LDPE to improve extrusion coating performance.Information provided b.. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D792 |
Dow FLEXOMER™ ETS-9064 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D792 |
Dow FLEXOMER™ ETS-9064 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Density | 0.911 g/cc @Temperature 23.0 °C |
0.0329 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group OREVAC® 18380 Maleic Anhydride Modified Polyethylene OREVAC® 18380 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D1505 |
Arkema Group Orevac® OE807 Maleic Anhydride modified LLDPE Orevac® OE807 resin is a maleic anhydride modified LLDPE designed for the coextrusion of multilayer barrier structures providing outstanding adhesion between the layers. Orevac® OE807 is characte.. |