Density 0.9287 - 0.9766 g/cc
0.03355 - 0.03528 lb/in³
7204 Cross-linker
Lord Adhesives Flocklok® 7000/7204 Flock Adhesive
LORD Flocklok® 7000/7204 adhesive is a two-part, single-coat adhesive used for adhering polyester or nylon flock fibers to a variety of thermoplastics, including PVC, Alcryn®, Sunprene®, ny..