Physical Properties Metric English Comments
Density 0.9375 g/cc
0.03387 lb/in³
ASTM D1505
Petromont 7000 Medium Density Polyethylene Resin
Petromont HDPE 7000 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is readily processed by blown sheet or flat die extrusi..
Density 0.9375 g/cc
0.03387 lb/in³
ASTM D792
Multibase Multi-Flex® TPE A 5401 BLK
Ash is 4.71%. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Density 0.9375 g/cc
0.03387 lb/in³
ASTM D1505
Petromont 7002 Medium Density Polyethylene Resin
Petromont HDPE 7002 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusi..