Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.9495 g/cc | 0.03430 lb/in³ | ISO 1183 |
Total Finathene® WR 201 B N HDPE blow molding
(discontinued **) FINATHENE® WR 201 B N is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® WR 201 B N has been developed for the blow molding of Plastic Fuel .. |
|||
Density | 0.9495 g/cc | 0.03430 lb/in³ | ISO 1183 |
Total Finathene® WR 201 B HDPE blow molding
(discontinued **) FINATHENE® WR 201 B is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® WR 201 B has been developed for the blow molding of Plastic Fuel Tan.. |