Physical Properties Metric English Comments
Density 0.965 g/cc
0.0349 lb/in³
ASTM D1505
Petromont 3000 High Density Polyethylene Resin
Petromont HDPE 3000 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is designed for injection moulding applications such as crates, cases, trays, tote bins and o..
Density 0.965 g/cc
0.0349 lb/in³
ASTM D4883
ExxonMobil Escorene® HD-6908 HDPE, Injection Grade  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Excellent Stiffness, Good ImpactUses: Crates, Pails, Industrial containers
Density 0.965 g/cc
0.0349 lb/in³
ASTM D4883
ExxonMobil HD 6908.18 Injection Molding Resin  (discontinued **)
HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requiring very high stif..
Density 0.965 g/cc
0.0349 lb/in³
ASTM D1505
LyondellBasell Alathon® H6030 High Density Polyethylene
ApplicationsALATHON H 6030 is a homopolymer that provides enhanced processability, excellent stiffness and short molding cycles. Typical applications include thin wall and deep-drawRegulatory Statu..
Density 0.965 g/cc
0.0349 lb/in³
ASTM D1505
LyondellBasell Alathon® M6580 High Density Polyethylene
ApplicationsALATHON M 6580 is a narrow molecular weight distribution homopolymer that enhances processability and stiffness, exhibits excellent color, low odor and good processing stability. Typica..
Density 0.965 g/cc
0.0348 lb/in³
Mixed
ITW Plexus Plexusâ„¢ MA425 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, long open time.Information provided by Illinois Tool Works.
Density 0.965 g/cc
0.0349 lb/in³
ASTM D792B; ISO 1183
Styron INSPIREâ„¢ TF1301 Thermoplastic Polyolefin
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010
Density 0.965 g/cc
0.0349 lb/in³
Solvay MACKAMINE® C-8 Surfactant
Product Description: Mackamine C-8 is a pure octyldimethylamine oxide that provides good wetting and very low foaming characteristics. It is compatible with most surfactants and because there are no..
Density 0.965 g/cc
0.0349 lb/in³
ASTM D1505
DuPont Elvax® 40W Ethylene-Vinyl Acetate Copolymer Resin
Elvax® 40W has a higher vinyl acetate content compared with the other Elvax® resins resulting in higher elongation, reduced hardness, improved solubility and adhesion, and significant differences ..
Density 0.965 g/cc
0.0349 lb/in³
ISO 1183
Borealis BS4641 High Density Polyethylene
BS4641 is a bimodal high-density polyethylene homopolymer. Because of its excellent organoleptic properties, this grade is especially suitable for blow molding of bottles for food applications. App..
Density 0.965 g/cc
0.0349 lb/in³
ExxonMobil method
ExxonMobil HDPE HD 6909.19 High Density Polyethylene Copolymer Resin
Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ..
Density 0.965 g/cc
0.0349 lb/in³
ExxonMobil method
ExxonMobil HDPE HD 6909.65 High Density Polyethylene Copolymer Resin
Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ..
Density 0.965 g/cc
0.0349 lb/in³
ExxonMobil method
ExxonMobil HDPE HD 7925.30 High Density Polyethylene Resin
Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.A..
Density 0.965 - 0.970 g/cc
0.0349 - 0.0350 lb/in³
BRCP 4843
ExxonMobil Jayflex™ DIDP Plasticizer
Appearance: Clear and FreeAvailability: AmericasCAS Number: 68515-49-1Information provided by ExxonMobil
Density 0.965 - 0.970 g/cc
0.0349 - 0.0350 lb/in³
BRCP 4843
ExxonMobil Jayflex™ DIDP-E Plasticizer
Appearance: Clear and FreeAvailability: AmericasCAS Number: 68515-49-1Information provided by ExxonMobil
Density 0.965 g/cc
0.0349 lb/in³
ASTM D792
Dow DMDA-8007 NT 7 High Density Polyethylene Resin
DOW DMDA-8007 NT is a narrow molecular weight distribution high density homopolymer designed to offer excellent stiffness, low warpage, good/acceptable toughness, and good mold-ability. This resin ..
Density 0.965 g/cc
0.0349 lb/in³
ASTM D792
Aclo Accutech Polypropylene Homopolymer HP0336W10L Wollastonite Reinforced
Density 0.965 g/cc
0.0348 lb/in³
Mixed
ITW Plexus Plexus™ MA925 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, long open time.Information provided by Illinois Tool Works.
Density 0.965 g/cc
0.0349 lb/in³
ASTM D792
Aclo Accutech TPO TPO030T9V Paintable Grade
Approved to Suzuki Spec Black B14257
Density 0.965 g/cc
0.0349 lb/in³
ASTM D1505
Amco PRIMATOP HDPE 006964EG Pipe Extrusion Polyethylene
HDPE 006964 features high quality for critical food packaging requirements and excellent stiffness. Applications include milk, water, and juice packaging.Former A-Top Polymers product; part of Amco ..