Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.9185 - 0.992 g/cc | 0.03318 - 0.0358 lb/in³ | Superior Quality |
Kazanorgsintez 153-02 K Polyethylene Composition for Cable Industry Production Method: Composition is achieved on the basis of high pressure polyethylene (low density) and low pressure (high density) with stabilizers and other additives. Application: Composition.. |