Physical Properties Metric English Comments
Density 1.0147 - 1.0149 g/cc
0.036658 - 0.036666 lb/in³
Solvay RHODISOLV® PORLARCLEAN Solvent
Description: Rhodiasolv PolarClean is a eco-friendly water soluble polar solvent or co-solvent very effective to solubilize agrochemicals. It is recommended to use in EC’s (emulsifiable concent..