Physical Properties Metric English Comments
Density 1.015 g/cc
0.03667 lb/in³
ACC EP Primer 59 EPI Engineered Polymer
EP Primer 59, “Powered by Reactamine® Technology”, is an ultra-fine, solvent-free Styrene modified acrylic-methacrylic-ester copolymer emulsion. It is suitable for both interior and exterior appl..