Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.037 - 1.047 g/cc | 0.03746 - 0.03783 lb/in³ | |
Kazanorgsintez Tert-butyl Prerbenzoate Production Method: Obtained by interaction of sodium salt of tertiary butyl hydro peroxide with benzoyl chloride. Application: Intended for use as a process initiator for production of LDPE, polysty.. |