Density 1.067 g/cc
0.03855 lb/in³
Melt; ISO 1183
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Conditioned)
Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla..
Density 1.067 g/cc
0.03855 lb/in³
Melt; ISO 1183
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla..