Physical Properties Metric English Comments
Density 1.076 g/cc
0.03887 lb/in³
ISO 1183
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66
PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures
Density 1.076 g/cc
0.03887 lb/in³
ASTM D4052
ExxonMobil Mobil Glygoyle 1000
Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T..
Density 1.076 g/cc
0.03887 lb/in³
ASTM D4052
ExxonMobil Mobil Glygoyle 460
Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T..
Density 1.076 g/cc
0.03887 lb/in³
ASTM D4052
ExxonMobil Mobil Glygoyle 680
Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T..
Density 1.076 g/cc
0.03887 lb/in³
226 g/m2; IEC 626
Dr. D. Mueller Flexiso® DMD FI 14010 00210 Polyester Electrical Insulation
Structure: Flexiso® DMD, FI 14010 00210 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with ..
Density 1.076 g/cc
0.03887 lb/in³
ASTM D4052
ExxonMobil Mobil Glygoyle 1000
Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T..
Density 1.076 g/cc
0.03887 lb/in³
ASTM D4052
ExxonMobil Mobil Glygoyle 460
Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T..
Density 1.076 g/cc
0.03887 lb/in³
ASTM D4052
ExxonMobil Mobil Glygoyle 680
Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T..