Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.121 g/cc | 0.04050 lb/in³ | |
Pyrotek Pyrocast AR LITE Castable Refractory A light weight highly insulating refractory product which offers excellent resistance to molten aluminum erosion and thermal shock.ApplicationsFor conveyance and casting of aluminum and its alloys A.. |