Polymer Property : Density = 1.122 g/cc
Polymer Property :
Density =
1.122 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
1.122
g/cc
0.04053
lb/in³
ISO 1183
Lanxess Durethan® BC 30 S 000000 Nylon 6
PA 6, non-reinforced, injection moldingInformation provided by LANXESS.