Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.206 g/cc | 0.04357 lb/in³ | ISO 1183 |
Lanxess Durethan® DP BM 410 H2.0 901510 Nylon 6, 10% Mineral + Glass Fiber PA 6, injection molding grade, 10% glass fibers/mineral, good heat-ageing resistance |
|||
Density | 1.206 g/cc | 0.04357 lb/in³ | ISO 1183 |
Lanxess Durethan® TP 140-009 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade, 15% glass fibers, elastomer-modified, good heat-ageing resistance, dry-impact modified |
|||
Density | 1.206 g/cc @Temperature 140 °C |
0.04357 lb/in³ @Temperature 284 °F |
|
Solvay Chemicals Glycerol alpha monochlorohydrin Viscous liquid used as chemical intermediate.EINECS Number: 202-492-4/CAS Number: 96-24-2/UN number: 2689Information provided by Solvay |