Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.224 g/cc | 0.04422 lb/in³ | ISO 1183 |
Stir SpA T 4599 A MOD (PVC) Application: Non-toxic transparent pipe for conveying waterInformation provided by STIR SpA |
|||
Density | 1.224 g/cc | 0.04422 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66 LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Density | 1.224 g/cc | 0.04422 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DX09301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Density | 1.224 g/cc | 0.04422 lb/in³ | JIS-Z-8807 |
Denka VINYKON S210060 PVC, S grade for transparent extrusion molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |