Physical Properties Metric English Comments
Density 1.354 g/cc
0.04892 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP PF008QS PA 6
LNP THERMOCOMP* PF008QS is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, Reduced Moisture.
Density 1.354 g/cc
0.04892 lb/in³
ISO 1183
BASF Ultramid® S3WG7 Balance 35% Glass Filled PA 610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Density 1.354 g/cc
0.04892 lb/in³
ISO 1183
BASF Ultramid® S3WG7 Balance 35% Glass Filled PA 610 (Dry)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..