Density 1.423 g/cc
0.05141 lb/in³
ISO 1183
Azoty Tarnow™ TARNOFORM 300 XEC1 POM
Electrically conductive, carbon fiber reinforced injection molding grade suitable for the applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe ..