Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.438 g/cc | 0.05195 lb/in³ | ISO 1183 |
Stir SpA RSN M 1 (PVC) Application: Molding for bends and connections, M-1 compliantInformation provided by STIR SpA |
|||
Density | 1.438 g/cc | 0.05195 lb/in³ | ISO 1183 |
Stir SpA SR 75 (PVC) Application: Extrusion pipe and sheath CEI 20-11 type TM-2Information provided by STIR SpA |
|||
Density | 1.438 g/cc | 0.05195 lb/in³ | ISO 1183 |
Stir SpA SG 88 OIL (PVC) Application: Extrusion insulating oil-proof sheath CEI 20-11 type R 2Information provided by STIR SpA |