Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.456 g/cc | 0.05260 lb/in³ | ISO 1183 |
Tisan TISAPET® 20% Glass Reinforced Polyethylene Terephthalate Properties:Excellent mechanical propertiesHigh thermal-chemical friction resistanceGood electrical propertiesGood rate of melt flow index relative to the quantity of glass fiberBalanced electrical a.. |
|||
Density | 1.456 g/cc | 0.05261 lb/in³ | |
Saint-Gobain Chemfab® q-GUARD® 112 Insulation Jacketing Description: q-GUARD® is a thermally durable and fire-safe composite developed specifically for use with removable and reusable insulation systems. Based upon PTFE fluorocarbon resins and fiberglas.. |