Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.486 g/cc | 0.05369 lb/in³ | JIS-Z-8807 |
Denka VINYKON R5020 PVC, R grade for hard extrusion A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Density | 1.486 g/cc | 0.05369 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF OF006I PPS - Linear LNP THERMOTUF* OF006I is a compound based on PPS - Linear resin containing Glass Fiber. Added features of this material include: High Impact. |