Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.506 g/cc | 0.05441 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP EX07305 PEI (Asia Pacific) Polyetherimide reinforced with Glass fiber and PTFE for use in Burn-in Test Sockets (BiTS) Application |