Polymer Property : Density = 1.700 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.700 g/cc
0.06140 lb/in³
CMT Materials PROTOBLOCK Air Permeable Prototype Tooling Material
PROTOBLOCK is a new composite material made of inorganic granules and epoxy resin engineered to form a micro-porous structure for use as prototype vacuum form or thermoform tooling. The material is..