Polymer Property : Density = 1.835 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density >= 1.835 g/cc
>= 0.06629 lb/in³
Solvay Sulfuric Acid Electrolyte Grade
Description: Sulfuric Acid electrolyte grade is colorless, clear and non-fuming with no visible sediment. It is very corrosive. The 93.2% strength solution complies with the Federal Specification O-..