Physical Properties Metric English Comments
Density 1.900 g/cc
0.06863 lb/in³
CMT Materials METAPOR® HD 210 AL Air Permeable Material
METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi..