Polymer Property : Density = 1.938 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.938 g/cc
0.07001 lb/in³
Pyrotek TS-114 Thermoset Electrical Insulation Product (Nema Grade: GPO-3)
Glass reinforcement, Polyester resin, Red color. Flame retardant. Excellent arc and track resistance. UL recognized.Information provided by Pyrotek.
Density 1.938 g/cc
0.07001 lb/in³
ISO 1183
Stir SpA IN 3340 AF PB (PVC)
Application: Extrusion flame resistant fillerInformation provided by STIR SpA