Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 12.37 g/cc | 0.4469 lb/in³ | |
American Elements Ruthenium Nanoparticles General DescriptionRuthenium (Ru) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Ruthenium Particles are typically 20 - 100 nanometers (nm) wi.. |