Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 15.6 g/cc | 0.564 lb/in³ | |
CMW® ELKONIUM 70 gold based alloy Pure gold has complete resistance to atmospheric tarnish and oxidation. It does not contribute to polymer formations like platinum and palladium alloys. Wrought gold metal is very soft and prone to .. |
|||
Density | 15.6 g/cc | 0.564 lb/in³ | |
Cadi 30WC Tungsten Copper Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |
|||
Density | 15.6 g/cc | 0.563 lb/in³ | |
Cadi Cu-Tungsten (80%) Copper Alloy Slightly higher tungsten content results in higher hardness and strength when forces are relatively high. Strength is gained with a slight decrease in electrical and thermal properties.Information .. |